Glossy Nuka Glaze is getting especially nice, if metal oxides cause color streaks (e.g. iron oxide or cobalt oxide).
56,2 Custer Feldspar
11,2 Talcum
11,2 Bone Ash
33,8 Flint
22,4 Whiting
11,2 Bentonite
37 Wood Ash
16,8 Frit 3134